Extruded Aluminum Heat Sink For Electronics
Aluminum extrusion heat sinks for power supplies, inverters, telecom units and control boards — 6063-T5 profiles up to 6,500 mm, machined and anodized in one factory, with the batch consistency and assembly data your production line needs.
- Product Introduction
An extruded aluminum heat sink for electronics is a finned aluminum profile produced by pushing heated 6063 or 6061 billet through a steel die, then cutting, machining and finishing it into a finished part. Because the base and fins come out of the die as one continuous piece of metal, there is no bond line or adhesive between them - the thermal path from the component to the fin tip is solid aluminum all the way. That is the reason extrusion remains the default cooling solution for power supplies, inverters, servo drives, telecom units and control boards, where heat loads are moderate and airflow is predictable.

Extrusion has a fixed cross-section along its length, which is both its advantage and its constraint. The advantage: one die serves every length you cut, so a single profile covers several product models and your unit cost drops with volume. The constraint: fin geometry is limited by what the die can produce - roughly 1.0 mm minimum fin thickness and an aspect ratio of about 10:1 in standard production. When a design needs thinner, denser fins, skiving is the better process, and we will say so rather than quote a profile that cannot be extruded.
We have produced extruded aluminum heat sinks for electronics in Foshan for 20 years, supplying OEM and ODM customers in Germany, Italy, Poland, the US and Canada. Our scope covers die design, extrusion, CNC machining, anodizing, inspection and export packing - so the part that arrives is finished and ready for your assembly line, not a raw profile waiting for three subcontractors.
Why Choose ZP HEAT SINK?
- 20 Years Extrusion & Export: Foshan factory since [Year], supplying electronics OEMs in the EU and North America.
- Finished Part, Not a Raw Profile: Die design, extrusion, CNC machining, anodizing and inspection under one roof - one supplier to hold accountable.
- Batch Data With Every Shipment: Material certificate, dimensional report and flatness measurement per lot, so incoming inspection is a comparison, not a guess.
- Honest Process Advice: If your fin geometry needs skiving or forging instead of extrusion, we say so before you pay for a die.
Product Specification
| Item | Specification |
| Material | Aluminum 6063-T5 (standard); 6061-T6 for structural parts; 1050A on request |
| Thermal Conductivity | 6063-T5 ≈ 200 W/m·K; 6061-T6 ≈ 167 W/m·K; 1050A ≈ 229 W/m·K |
| Process | Extrusion+cut to length+CNC machining+anodizing |
| Profile Width | 10 mm - 300 mm |
| Profile Height | 5 mm – 150 mm (base + fin) |
| Max Cut Length | 6500 mm |
| Fin Thickness | 1.0 mm minimum (standard); 0.8 mm achievable with special die design |
| Fin Aspect Ratio | Up to 6:1 standard; 10:1 practical maximum for 6063-T5 |
| Min Fin Gap | 1.2 mm (below this, die life and extrusion speed drop sharply) |
| Base Thickness | 2 mm-12mm |
| Profile Tolerance | Base ±0.3 mm, fin thickness ±0.2 mm, overall ±0.5 mm (EN 755-9 basis) |
| Machined Flatness | ≤ 0.1 mm standard; ≤ 0.05 mm on machined contact faces |
| Surface Finish | Clear anodized 8-12 μm; black anodized 15-20 μm; chromate; bare mill finish |
| Typical Applications | Power supply, inverter, servo drive, telecom unit, control board, LED driver |
| MOQ | 100 pcs from an existing profile; 500 kg for a new die |
Product Gallery


Product Application

- Switching power supplies and adapters: 50 W to 500 W AC/DC supplies, DIN-rail power units and LED drivers. Straight-fin extrusion with a 6-8 mm fin gap suits the natural convection inside a closed metal case.
- Inverters and motor drives: Solar inverters, VFDs and servo drives. Long profiles run the length of the enclosure and double as the mounting rail, keeping the IGBT or MOSFET bank at a uniform temperature.
- Telecom and network equipment: Remote radio units, switches and power distribution shelves. Anodized extrusion withstands outdoor humidity and keeps the surface electrically insulating where required.
- Industrial control and instrumentation: PLCs, IO modules, analyzers and laboratory instruments. Small flat-back profiles with machined holes fit standard DIN and rack formats.
- LED drivers and lighting electronics: Driver housings with integral fins, where the extrusion serves as both the enclosure and the cooling surface - see Module IG-4 for the structural case.
- Medical and laboratory power electronics: Compact supplies where the heat sink must be anodized for electrical isolation and the finish cannot shed particles into the enclosure.
Why an Approved Sample Does Not Guarantee an Approved Batch
Almost every extrusion heat sink project follows the same sequence: you receive a sample, you measure it, you approve it, and you place a production order. What the sample proves is that the process can make one good part on the day it was made. What it does not prove is that part number 5,000 will measure the same - and that difference is where most incoming-inspection disputes start.
Three things drift between the first article and a later batch, and all three change thermal performance:
- Fin thickness tolerance: Extruded fin thickness carries roughly ±0.2 mm. On a nominal 1.5 mm fin, a batch running at 1.7 mm has about 13% less fin surface per unit width and slightly wider gaps. At the same airflow the thermal resistance moves by a few percent - enough to fail a tight acceptance criterion, not enough to be visible on a drawing.
- Die wear: A new die produces sharp, full-height fins. As the die wears, fin roots thicken and fin tips become less defined, and the effective fin height drops. A die that has run 20,000 kg and one that has run 8,000 kg do not produce identical profiles, even from the same drawing.
- Straightness and cut-length drift: Long profiles bow during quenching and handling. Straightness, not thickness, is usually the dimension that fails first on a long electronics heat sink, and it affects how the part seats against a chassis or a clamp.
How we control it
- A first-article inspection report that states the measured fin thickness, gap, base thickness and flatness - not just "passed".
- A retained golden sample per die, kept on file, used as the visual and dimensional reference for every repeat order.
- Lot-level dimensional sampling on fin thickness, fin height and base flatness, reported with the shipment so your incoming inspection has something to compare against.
- Die life tracking by extruded weight, with die replacement flagged before fin definition degrades into the tolerance band.
The Assembly Tolerance Stack: Flatness, Interface Thickness and Clamp Force
A heat sink drawing usually specifies the contact-face flatness and stops there. But the thermal resistance the assembly actually delivers is set by three variables acting together: how flat the base is, how thick the thermal interface layer ends up being, and how evenly the part is pressed against the heat source. Each one is individually within tolerance in most designs, and the combination is still worse than the thermal budget assumed.
The stack-up, in numbers:
| Variable | Typical value | What it does to the thermal |
| Base flatness | 0.05-0.10 mm on a machined face | Sets the minimum gap the interface must fill at the worst point |
| Interface material | 0.2 mm pad, or 0.05 mm grease layer after compression | A pad is roughly 4× thicker than a compressed grease layer, and adds resistance accordingly |
| Clamp force and its distribution | Single screw at the centre vs four screws at the corners | One screw tilts the base; corner screws hold it parallel but can bend a thin base |
| Post-assembly gap | 0.25 – 0.35 mm worst case with a pad and one centre screw | The gap the thermal path actually sees, not the 0.2 mm printed on the pad datasheet |
Two practical consequences. First, a thin heat source footprint on a wide base needs a spread analysis, not just a flatness tolerance - heat has to travel laterally through the base before it reaches the fins, and on a 3 mm base that spreading resistance can be a significant share of the total.
Second, if your assembly uses a single central screw on a part longer than about 80 mm, the base will tilt and the interface layer will be thicker at the ends than under the screw. Four corner screws, or a central screw plus a machined step, holds the gap uniform.
What we do about it on the part: machine the contact face after extrusion rather than relying on as-extruded flatness, control flatness to 0.05 mm where a pad is used, keep the machined face free of anodizing so the thermal path does not run through an oxide layer, and mark the datum and the contact area explicitly on the drawing so your assembly station knows which surface is the thermal one.
What you should do about it on the design side: decide the interface material before the flatness callout, not after. A 0.2 mm pad needs a different flatness spec than a compressed grease layer, and specifying 0.05 mm flatness for a design that will use a thick gap-filling pad buys cost without buying performance.
Why Two Quotes for the Same Drawing Differ by 100%
Send one drawing to three extrusion suppliers and the quotes can come back at $2.10, $3.40 and $5.80 per piece. Nobody is necessarily lying. The difference is in what each price includes, and those inclusions are exactly the things that decide whether the parts work in your assembly. It is worth knowing which lever is moving before you compare the totals.
| Price lever | What varies | What it means for you |
| Alloy actually used | 6063-T5 at 200 W/m·K vs a lower-grade or recycled billet | Lower conductivity is compensated by a bigger profile - or not compensated at all |
| Die age and owndership | Amortised new die vs. an old die the supplier already owns | An old die means thicker fins and less consistent sections; the die cost may simply be hidden |
| Tolerance regime | As-extruded vs. machined contact face | As-extruded flatness on a long profile is typically 0.3-0.5mm, not the 0.1 mm on the drawing |
| Anodizing | In-house vs. outsourced vs. none | Outsourced anodizing adds freight, a second lot to trace, and 3-5 days |
| Inspection | Full dimensional report per lot vs. visual check only | The report is the labour content of incoming-inspection disputes |
| Packing | Bulk bundles vs. ends protected, anti-scratch wrap, marked cartons | Unprotected long profiles arrive bowed or scratched; the rework lands on your line |
| Yield allowance | Quoted against 100% good parts vs. quoting a price that assumes 92% | The low quote may be pricing t he scrap risk into your incoming reject rate. |
A useful habit: ask every supplier to quote the same scope in writing - material grade and temper, cut length, machining operations, finish type and thickness, inspection report, packing method, and tooling shown separately from the unit price. Once those seven lines are on the comparison sheet, the spread usually collapses to a defensible range, and the remaining difference is capacity, geography or margin - which are fair reasons to choose one supplier over another.
One more line worth adding: ask what happens if the first lot fails your incoming inspection. A supplier who answers with a replacement policy and a measurement method is quoting a relationship. A supplier who answers with silence is quoting a shipment.

When the Heat Sink Is Also the Enclosure
In a large share of electronics projects the extrusion is not only a heat sink - it is the device's housing, mounting rail or chassis. This is common in LED drivers, DIN-rail power supplies, outdoor telecom units and industrial sensor enclosures. Combining the two functions saves a part, a fastener set and an assembly step, but it also means the profile is being optimised for three jobs at once, and they pull against each other.
| Function | What it wants | Where it conflicts with the others |
| Thermal | Maximise fin area and fin height | Fin area wants height; a housing wants a compact, grippable outline |
| Mechanical | Wall thickness, screw bosses, impact and vibration resistance | Thicker walls and bosses consume section width that would otherwise be fin |
| Electrical / EMC | Isolation between the heat sink and live parts; grounding path if used as s shield | Anodizing inslates the surface, so a grounding path needs a masked or machined contact area |
| Ingress protection | Sealed ends, gasket grooves, IP-rated joints | Closed channels and end caps trap heat-the enclosure that protects also insulates |
| Manufacturing | One die, one extrusion, one finish | A complex combined section raises die cost and lowers extrusion speed |
Four practical rules we apply when a profile has to do both jobs. Keep the fin field on one side and the mounting or gasket features on the other, so the thermal and mechanical functions do not share section width. Specify a masked contact area if the heat sink must provide a grounding path - anodizing is an insulator and a 15 μm layer will fail a continuity test. Treat a sealed enclosure as a thermal problem in its own right: the internal air temperature rises above ambient, so size the fins against internal air, not room temperature. And accept that a combined profile will extrude slower than a pure heat sink section - that cost belongs in the quotation, not in a surprise at the first shipment.
If your project needs extreme fin density and a sealed housing at the same time, the honest answer is usually two parts: an extruded housing with modest fins, plus a skived or forged heat sink mounted inside. We will price both routes so you can compare total assembly cost, not just the piece price of one profile.
Long-Term Reliability: Warpage, Thermal Cycling and Interface Degradation
A heat sink that meets its thermal target on day one can still fail the product in year three. Three degradation mechanisms matter in electronics assemblies, and each has a design or process answer that costs little if it is designed in and a great deal if it is discovered in the field.
Warpage after machining and anodizing. Long, thin profiles bow when material is removed from one side or when the anodizing bath changes the surface stress balance. A base that was flat at machining can be 0.2-0.3 mm out of flat after finishing, which silently thickens the interface layer. Answer: machine and finish in the order that leaves the base flat, inspect flatness after finishing rather than before, and keep the profile symmetric where the drawing allows it.
Thermal cycling fatigue at the interface. Repeated heating and cooling causes the interface material to expand and contract more than the aluminum. Over thousands of cycles, grease is pumped out of the contact area and pads can compress permanently - a phenomenon usually called pump-out. The thermal path degrades while the part still looks fine. Answer: choose phase-change materials or a pad with a controlled thickness for high-cycle applications, avoid designs that rely on a very thin grease layer under high clamp pressure, and validate with a cycling test rather than a single steady-state measurement.
Mechanical stress transferred to solder joints. A heavy heat sink clamped to a small package puts the solder joints under constant load, and thermal expansion adds a cyclic component. This is a packaging problem, not a heat sink problem, but the heat sink mass and the mounting method are the two levers that control it. Answer: keep the heat sink mass proportional to the package, use a compliant mounting arrangement or a spring-loaded clip rather than a rigid screw stack, and confirm the mounting load against the device's mechanical limits before fixing the clamp design.
For projects where long-term stability is a stated requirement - outdoor telecom, automotive adjacent, medical - tell us at RFQ stage. We can supply flatness measured after finishing, run a thermal cycling screening on prototypes, and specify the interface material together with the heat sink so the two are validated as one assembly instead of two parts bought from two suppliers.
FAQ
Q: What is the difference between an extruded and a skived aluminum heat sink?
A: Extrusion forms the fins by pushing metal through a die, so fin thickness is limited by die strength - about 1.0 mm minimum in standard production, with an aspect ratio ceiling around 10:1. Skiving slices fins from a solid billet, reaching 0.05 mm fins and far higher fin density in the same volume, at a higher unit cost and with less freedom in profile shape. Use extrusion for cost-sensitive designs with predictable airflow and moderate heat flux; use skiving when the enclosure is small and the heat load is high.
Q: Which alloy should I specify - 6063, 6061 or 1050?
A: 6063-T5 is the default for heat sinks: it extrudes fast, takes a good anodized finish and conducts about 200 W/m·K. 6061-T6 is stronger (roughly 240 MPa yield versus 170 MPa) but conducts about 167 W/m·K, so it is chosen when the heat sink is also a structural bracket - expect a 10-15% surface-area penalty to compensate. 1050A conducts about 229 W/m·K but is too soft for tall fins, so it suits low-profile LED heat sinks where thermal demand dominates.
Q: Why does my 0.1 mm flatness callout not give the thermal performance I calculated?
A: Because flatness is only one of three variables. The installed thermal resistance is set by flatness, by how thick the interface layer actually ends up after clamping, and by how evenly the clamp force is distributed. A single central screw on a long part tilts the base, so the interface is thicker at the ends than under the screw. Four corner screws, or a machined step, keeps the gap uniform. See Module IG-2 for the stack-up.
Q: Can the heat sink be anodized and still provide an electrical ground path?
A: Not on the anodized surface. Anodizing is an insulating oxide layer - 8-20 μm is enough to fail a continuity test. If the heat sink must carry a ground path, specify a masked area or a machined contact pad that stays bare metal, and show it on the drawing so the finishing shop knows to mask it before anodizing.
Q: What is the minimum order quantity and what does tooling cost?
A: From an existing profile, MOQ is 100 pcs and there is no tooling cost. A new die has an MOQ around 500 kg of extruded output; simple single-cavity dies typically run a few hundred to a few thousand dollars depending on section complexity and width, with 20-30 days for design, cutting and trial extrusion. We quote tooling separately from the unit price so you can see what is one-time and what is per part.
Q: How do you handle long profiles that arrive bent or scratched?
A: By specifying the packing before the order, not after the claim. Long profiles are bundled with end protection, wrapped against abrasion, and loaded so the bundle is supported along its length rather than cantilevered. Straightness is inspected before packing and stated on the inspection report. If your receiving process requires a tighter straightness limit than the extrusion standard, tell us at RFQ - it is cheaper to control at the press than to rework after freight.
Hot Tags: extruded aluminum heat sink for electronics, China, suppliers, manufacturers, factory, customized, wholesale, buy, price, free sample, aluminum cooler, Aluminum Extruded PCB Heat Sink, aluminum extrusion enclosure, CNC machined heatsink, custom heatsink, heat sink profile
You Might Also Like